He ammonium polyphosphate ʻo TF-201S me ka nui o nā ʻāpana maikaʻi loa, ka solubility wai haʻahaʻa a me ke kūpaʻa kiʻekiʻe. Loaʻa iā ia nā ʻano o ka viscosity haʻahaʻa a me ke kiʻekiʻe o ka polymerization, a ʻaʻohe mea ʻawahia a pili i ke kaiapuni.
Ma ke ʻano he "mea hāʻawi waikawa" o nā uhi hoʻonui lapalapa, kūpono loa ʻo TF-201S no nā uhi pale ahi, a ua hoʻokō ʻia kona kumumanaʻo pale ahi ma o ka ʻōnaehana hoʻonui.
I ke ana wela kiʻekiʻe, e palaho ʻo TF-201S i loko o ka waikawa phosphoric polymeric a me ka ammonia. Hoʻopili ka waikawa Polyphosphoric me nā hui hydroxyl e hana i nā esters phosphate paʻa ʻole. Ke hōʻike ʻia i nā lapalapa, e hana ka uhi pale ahi i ka huʻa carbonaceous, e pale pono ana i ka hopena o ka piʻi ʻana o ka mahana ma luna o ka substrate.
Ma ke ʻano o ka pale ʻana i ka lapalapa o ka laholio, ua maopopo loa ka hopena o TF-201S. Ua hoʻopili pono nā mea kūʻai aku iā TF-201S i ka mālama ʻana i ka pale ʻana i ka lapalapa o nā kāʻei conveyor me nā hopena maikaʻi loa.
He pauka keʻokeʻo ʻo TF-201S, kūpono no nā ʻano mea he nui, e like me nā uhi ʻana, nā mea hoʻopili, nā kaula, a pēlā aku.
1. Hoʻohana ʻia e hoʻomākaukau i nā ʻano ʻano uhi intumescent kiʻekiʻe, ka lāʻau pale ahi no ka lāʻau, hale papa nui, moku, kaʻaahi, nā kaula, a pēlā aku.
2. Hoʻohana ʻia ma ke ʻano he mea hoʻohui flameproof nui no ka mea hoʻonui lapalapa ʻano hoʻonui i hoʻohana ʻia i loko o ka plastic, resin, rubber, etc.
3. E hana i mea kinai pauka e hoʻohana ʻia ma ke ahi ākea no ka ululāʻau, ke kahua ʻaila a me ke kahua lanahu, a pēlā aku.
4. I loko o nā palakiko (PP, PE, a me nā mea ʻē aʻe), Polyester, Rubber, a me nā uhi pale ahi hiki ke hoʻonui ʻia.
5. Hoʻohana ʻia no nā uhi lole.
| Nā kikoʻī | TF-201 | TF-201S |
| helehelena | Pauka keʻokeʻo | Pauka keʻokeʻo |
| P2O5(w/w) | ≥71% | ≥70% |
| Huina Phosphorus (w/w) | ≥31% | ≥30% |
| ʻIke N (w/w) | ≥14% | ≥13.5% |
| Ka Mahana Hoʻopau (TGA, 99%) | >240℃ | >240℃ |
| Ka hoʻoheheʻe ʻia (10% aq., ma 25ºC) | <0.50% | <0.70% |
| ka waiwai pH (10% aq. Ma 25ºC) | 5.5-7.5 | 5.5-7.5 |
| Ka mānoanoa (10% aq, ma 25 ℃) | <10 mpa.s | <10 mpa.s |
| Ka makū (w/w) | <0.3% | <0.3% |
| Ka nui o ka ʻāpana awelika (D50) | 15~25µm | 9~12µm |
| Ka nui o nā ʻāpana (D100) | <100µm | <40µm |